Availability: | |
---|---|
Quantity: | |
XM-BA13
XIMI
Natural Barite Powder Price XM-BA13 In the composite system of PA66 modified by melt grafting maleic anhydride with 20% activated barium sulphate and 5% ethylene octyl copolymer, a small part of barium sulphate has the effect of heterogeneous nucleation on PA66, and most of barium sulfate has the effect of toughening PA66.
SPECIFICATION | ||
Apperance | White Powder | |
D50 (μm) | max | 1.5 |
BaSO4 content (%) | 98.5 | |
Volatile matter (105℃) | max | 0.2 |
Whiteness (%) | min | 96.5 |
Oil Absorption g/100g | 16~20 | |
Ph Value | 7.3~8.6 | |
Specific Gravity g/cm3 | 4.2~4.3 | |
Water Soluble Matters (%) | max | 0.06 |
Refraction Index | 1.64 | |
Iron Fe (%) | max | 0.003 |
Electrical Conductivity (Us/cm) | max | 150 |
Natural Barite Powder Price XM-BA13 In the composite system of PA66 modified by melt grafting maleic anhydride with 20% activated barium sulphate and 5% ethylene octyl copolymer, a small part of barium sulphate has the effect of heterogeneous nucleation on PA66, and most of barium sulfate has the effect of toughening PA66.
SPECIFICATION | ||
Apperance | White Powder | |
D50 (μm) | max | 1.5 |
BaSO4 content (%) | 98.5 | |
Volatile matter (105℃) | max | 0.2 |
Whiteness (%) | min | 96.5 |
Oil Absorption g/100g | 16~20 | |
Ph Value | 7.3~8.6 | |
Specific Gravity g/cm3 | 4.2~4.3 | |
Water Soluble Matters (%) | max | 0.06 |
Refraction Index | 1.64 | |
Iron Fe (%) | max | 0.003 |
Electrical Conductivity (Us/cm) | max | 150 |